Description

SBR 1712

Styrene Butadiene Rubber

Item Unit Specification Result Test Method
Raw Mooney Viscosity MU 42-52  

47

ASTM D1646-07
Volatile Matter Content % Max 0.75  

0.5

ASTM D5668-09
Ash Content % Max 1.00  

0.19

ASTM D5667-95
Soap Content % Max. 0.50  

0.15

ASTM D5774-95
Organic Acid % 3.9 – 5.70  

4.9

ASTM D5774-95
Bound Styrene % 22.5 – 24.5  

23.5

ASTM D5775-95
Compound Properties (ASTM D 1646-03) – ( ML 1+4@ 100° C)1
Compound Mooney

Viscosity

MU Max 62 58 ASTM D1646-07
Tensile Strength,

35 min at 145° C cured

kg/cm² min 200 235 ASTM D412-06
Elongation at Break,

35 min at 145°C cured

% min 530 617 ASTM D412-06
300% Modulus,

35 min at 145°C cured

 

kg/cm²

 

79 – 109

 

87

 

ASTM D412-06